Effect of Air Abrasion on the Marginal Configuration of Titanium Crowns after Casting

Ramesh Nadiger, Bhupender Yadav, Puja Malhotra, Harish Yadav

Citation Information : Nadiger R, Yadav B, Malhotra P, Yadav H. Effect of Air Abrasion on the Marginal Configuration of Titanium Crowns after Casting. Int J Prosthodont Restor Dent 2013; 3 (4):131-135.

DOI: 10.5005/jp-journals-10019-1092

Published Online: 01-12-2013

Copyright Statement:  Copyright © 2013; Jaypee Brothers Medical Publishers (P) Ltd.


Abstract

How to cite this article

Yadav B, Malhotra P, Nadiger R, Yadav H. Effect of Air Abrasion on the Marginal Configuration of Titanium Crowns after Casting. Int J Prosthodont Restor Dent 2013;3(4):131-135.


PDF Share
  1. Effect of air abrasives on marginal configurations of porcelain fused to metal alloys: an SEM analysis. J Prosthet Dent 1991;65:38-43.
  2. Microabrasion of cast metal margins—awarning. J Prosthodont 2007;16:136-140.
  3. Adherence of a nickelchromium alloy and porcelain. J Prosthet Dent 1979;41: 167-172.
  4. Effect of varying surface texture on bond strength of one semiprecious and one nonprecious ceramoalloy. J Prosthet Dent 1979;42:86-95.
  5. New method for divesting cobaltchromium alloycastings: sandblasting with a mixed abrasive powder. J Prosthet Dent 2001;85:357-362.
  6. Effect of sandblasting and silica coating on dental alloys: volume loss, morphology and changes in the surface composition. Dent Mater 1993;9:155-161.
  7. Titanium for prosthodontic applications: A review of literature. Quintessence Int 1996;27:401-408.
  8. Effect of surface contamination on adhesive bonding of cast pure titanium an Ti-6Al-4V alloy. J Prosthet Dent 1999;81:270-276.
  9. Effect of sandblasting and silica coating procedures on pure titanium. J Dent 1994;22:300-306.
  10. surface roughness and fatigue performance of commercially pure titanium and Ti-6Al-4Valloy after different polishing protocols. J Prosthet Dent 2005;93:378-385.
  11. Effect of different finishing and polishing agents on the surface roughness of cast pure titanium. J Prosthodont 2007;16:263-268.
  12. surface roughness and fatigue performance of commercially pure titanium and Ti-6Al-4 Valloy after different polishing protocols. J Prosthet Dent 2005;93:378-385.
  13. Effect of metal design on marginal distortion of metal ceramic crowns. J Dent Res 1984;63: 1327-1331.
PDF Share
PDF Share

© Jaypee Brothers Medical Publishers (P) LTD.